BS EN 10210 specifies technical delivery condition for hot finished circular, square or rectangular hollow sections and applies to hollow sections for hot, with or without subsequent heat treatment, or formed cold with subsequent heat treatment to obtain equivalent metallurgical conditions to those obtained in the hot formed product.

Simone Woods

Simone Woods

Simone Woods

Range

C

Mn

P

S

N

Al

CEV

min

-

-

-

-

-

0.020

-

max

0.17

1.40

0.040

0.040

0.009

-

0.37

Impact Value

Tensile Strength

Impact Test Temp.

Elongation

Yield Strength

min

27 J

52 Ksi [360 MPa]

20°C [68°F]

26 %

34 Ksi [235 MPa]

max

-

74 Ksi [510 MPa]

-

-

-