Hot finished structural hollow sections / tubes of non-alloy and fine grain steels
32-4340.JPG

BS EN 10210 specifies technical delivery condition for hot finished circular, square or rectangular hollow sections and applies to hollow sections for hot, with or without subsequent heat treatment, or formed cold with subsequent heat treatment to obtain equivalent metallurgical conditions to those obtained in the hot formed product.

Simone Woods

Simone Woods

Simone Woods

Range

C

Mn

P

S

Al

CEV

min

-

-

-

-

0.020

-

max

0.20

1.50

0.030

0.030

-

0.41

Yield Strength

Impact Test Temp.

Impact Value

Elongation

Tensile Strength

min

40 Ksi [275 MPa]

-20°C [-4°F]

27 J

23 %

62 Ksi [430 MPa]

max

-

-

-

-

84 Ksi [580 MPa]